The produc has excellent electrical insulation properties, is widely used in the recovery of the main insulation layer of 36 kV and below power cables joints, and other places where require insulation.
Features.-
-
Material: polyolefin, cross linked polymeric inner.
-
Operating temperature: -45 oC ~ 105 oC.
-
Shrink temperature: start at 100 oC and shrink totally at 130 oC.
-
Standard color: red.
Dimensions
|
Part No. |
Diameter (mm) |
recovered wall
thickness Nom. (mm) |
standard lenght (mm) |
As supplied
Min. (mm) |
After recovery
Max. (mm) |
WRSHJG-30/12 |
30 |
12 |
3.7 |
500 - 850 |
WRSHJG-35/14 |
35 |
14 |
4.0 |
500 - 850 |
WRSHJG-40/17 |
40 |
17 |
4.0 |
500 - 850 |
WRSHJG-45/18 |
45 |
18 |
4.0 |
500 - 850 |
WRSHJG-50/22 |
50 |
22 |
4.0 |
500 - 850 |
WRSHJG-55/25 |
55 |
25 |
4.0 |
500 - 850 |
WRSHJG-55/22 |
55 |
22 |
5.5 |
500 - 850 |
WRSHJG-60/25 |
60 |
25 |
6.0 |
500 - 850 |
WRSHJG-65/26 |
65 |
26 |
6.0 |
500 - 850 |
WRSHJG-70/29 |
70 |
29 |
6.0 |
500 - 850 |
WRSHJG-80/35 |
80 |
35 |
6.0 |
500 - 850 |
WRSHJG-85/36 |
85 |
36 |
6.0 |
500 - 850 |
WRSHJG-90/38 |
90 |
38 |
6.0 |
500 - 850 |
WRSHJG-100/42 |
100 |
42 |
6.0 |
500 - 850 |
Technical Data
|
Property |
Test Method |
Standard Value |
Operating temperature |
IEC 216 |
- 45 oC to + 105 oC |
Tensile strength |
ASTM-D 2671 |
≥ 12 MPa |
Elongation at break |
ASTM-D 2671 |
≥ 300% |
Tensile strength after aging |
ASTM-D 2671/130 oC, 168 hrs |
≥ 10 MPa |
Elongation at break after aging |
ASTM-D 2671/130 oC, 168 hrs |
≥ 250% |
Dielectric strength |
IEC 243 |
≥ 25 kV/mm |
Volume resistance |
ASTM-D 2303 |
≥ 1x1015 Ω.cm |
Dielectric constant |
IEC 250 |
3.0 |
Longitudinal shrinkage |
- |
≤ 10% |
Eccentricity |
ASTM-D 2671 |
≤ 30% |
Water absorption |
ISO 62 |
≤ 0.1% |
Copper corrosion |
ASTM-D 2671 |
120 oC, 168 hr, no corrosion |
Cold bend |
ASTM-D 2671 |
- 40 oC, 4 hr, no cracking |